| Properties | Value |
|---|---|
| Carbon | 0.14-0.19 |
| Silicon | 0.40 max |
| Sulphur | 0.035 |
| Manganese | 1.00-1.30 |
| Phosphorous | 0.035 |
| Chromium | 0.80-1.10 |
Mechanical properties of 16MnCr5 EFW tube
| Properties | Value | |
|---|---|---|
| Yield strength | MPa | > 600 |
| Tensile strength | 880-1230 | |
| Elongation | % | 9 |
| Hardness | HB | < 207 |
Physical properties of DIN 17210 Tube
| Properties | Value | |
|---|---|---|
| Youngs module | GPa | 210 |
| Shear module | 80 | |
| Density | kg/m3 | 7800 |
| Average CTE 20-300°C | µm/m°K | 12 |
| Poisson´s ratio | - | 0.3 |
| Specific heat capacity 50/100°C | J/kg°K | 460 - 480 |
| Thermal conductivity | W/m°K | 40 - 45 |
| Electrical resistivity | µΩm | 0.20 - 0.25 |
DIN 17210 Gr 16MnCr5 CS SMLS tube thermal properties
| Property | Coefficient of thermal expansion | ||||||||
|---|---|---|---|---|---|---|---|---|---|
| Temperature | °C | -100.0 | 20.0 | 100.0 | 200.0 | 300.0 | 400.0 | 500.0 | 600.0 |
| Value | 1/K | 1.05E-5 | 1.15E-5 | 1.1E-5 - 1.21E-5 | 1.27E-5 | 1.32E-5 | 1.36E-5 | 1.4E-5 | |
DIN 17210 welded tube specific heat capacity
| Specific heat capacity | ||||||||
|---|---|---|---|---|---|---|---|---|
| °C | -100.0 | 20.0 | 100.0 | 200.0 | 300.0 | 400.0 | 500.0 | 600.0 |
| J/(kg·K) | 423 | 460 - 461 | 479 | 499 | 517 | 536 | 558 | 587 |
| China | GB | 15CrMn/ 16MnCr/20CrMnTi |
|---|---|---|
| Russia | GOST | 18KHG |
| France | AFNOR | 16MC5 |
| England | BS | 527M17/ 590M17 |
| EU | EN | 16MnCr5 |
| Italy | UNI | |
| Spain | UNE | |
| Inter | ISO | |
| Germany | DIN,WNr | |
| Sweden | SS | 2127 |
| USA | - | SAE5115 |
| Poland | PN | 15HG |
| Czechia | CSN | 14220 |
Hardness range of 16mncr5 CS seamless tube
| Properties | Value | ||
|---|---|---|---|
| Vickers hardness | HV | +A | 170 |
| Brinell hardness | HBW | +A | 207 |
| +TH | 156 - 207 | ||
| +FP | 140 - 187 | ||
| +N | 138 - 187 | ||
| Rockwell B hardness | HRB or RB | +A | 84 |
DIN 17210 Grade 16MnCr5 EFW tube heat treatment
| Treatment | Condition | Cooling/quenching | Temperature°C |
|---|---|---|---|
| Hot forging | +U | Slow or in air | 850-1200 |
| Normalizing | +N | In air | 860-890 |
| Stress relieve annealing | +SRA | 600-680 | |
| Carburizing | +C | 880-980 | |
| Tempering | +T | 150-200 | |
| Soft annealing | +A | Slowly (15°C/h) until 600°C | 670-710 |
| Quenching | +Q | In oil or water | 860-900 |